Hello,
I have been using the GSAS software to analyse some XRD data from MgH2
samples that have been heavily milled.
One piece of information I would like to assertain is the mean particle
size of my powders. The powders are of the order of 10 nm by TEM.
Some relevant information;
I am using a type 2 profile function.
My data is horrible with very broad peaks of very low intensity.
I have had to set the GU GV and GW parameters in order to do anything at
all. If I let them float then I lose any semblance.
I get a Chi2 < 1.
My question is this;
How do I obtyain the particle size?
Is it the LX parameter and is this measured in Angstroms?
I hope someone will be kind enough to help me out of this mire!
Regards
Dave Weston
Research Fellow
Department of M3
Wolfson Building
University of Nottingham
This message has been checked for viruses but the contents of an attachment
may still contain software viruses, which could damage your computer system:
you are advised to perform your own checks. Email communications with the
University of Nottingham may be monitored as permitted by UK legislation.