rietveld_l  

Re: Negative Biso / absorption in TOPAS.

Lubomir Smrcok
Wed, 10 Feb 2010 01:32:52 -0800

Jacco,
could you kindly tell us the composition of the sample and the technique used to collect the data ?
Lubo


On Wed, 10 Feb 2010, Jacco van de Streek wrote:

Dear colleagues,

I am helping some people from the University of Frankfurt with their
Rietveld refinements, and usually their powder patterns are measured on
their own instrument and the refinements are excellent. This time,
however, they have to work with a powder pattern that was sent to them.
It is laboratory X-ray data, copper radiation, visible peaks out to 60
degrees 2theta, reasonable counting statistics, almost certainly flat
plate (reflection). The crystal structure is known. For the refinement,
they have TOPAS available.

The Rietveld refinement progresses very smoothly, but when the global
Biso is refined, it becomes very large and negative (-4). If we allow
the Biso to become negative, the difference curve is a flat line, in
other words, the fit is perfect. If we fix the global Biso at, say, 3.0,
the fit is still very good, but not as good as we are used to and the
difference curve starts to show some small residuals. We have no
experience with this, but some Google searches suggest "absorption" as
the problem. We have already modelled anisotropic peak broadening and in
our experience the background is modelled very well in TOPAS and does
not correlate with other parameters.

So our main two questions are:

1. Is absorption indeed the most likely cause of this problem or are
there other possibilities?

2. How do we model absorption in TOPAS? Which keyword do we use and what
are reasonable values for the parameters in the expression?

Best wishes,
--
Dr Jacco van de Streek
Senior Scientist
Avant-garde Materials Simulation