rietveld_l  

Re: Intrumental broadening of 2D detector

Franz Werner
Fri, 19 Feb 2010 01:06:42 -0800

Hello Wing

> I'm unable to get NIST 660 because they have been out of stock for a few
> months

As described by D. Balzar et al. (http://dx.doi.org/10.1107/S0021889804022551), 
annealed CeO2 is an equivalent alternative.

Franz Werner
--
Tallinn University of Technology
Department of Chemistry
-- 
GRATIS für alle GMX-Mitglieder: Die maxdome Movie-FLAT!
Jetzt freischalten unter http://portal.gmx.net/de/go/maxdome01