Dear Shishir Ray,

in the current release of "Pearson's Crystal Data" (http://www.crystalimpact.com/pcd ), there are 29 entries that match your criteria, describing seven different orthorhombic phases. 10 entries originate from papers that were published in 2005 or later.

Best regards
Holger Putz

Am 11.03.2010 um 21:09 schrieb sisir ray:

Dear Rietveld community,
I am looking for the latest *.cif files for RMnO3 (R = Sm,Eu,Gd,Dy,Ho,Yb) compounds in orthorhombic and hexagonal phases .Can any body suggest where I can find them.
I really appreciate the help.