Dear Rietveld users,
We are currently using transmission flat sample on our diffractometer.
To prepare the transmission flat sample we are using mylar 15microns or
kapton. We put the sample between 2 mylar foils.
I would like to know if there is some tricks in order to nicely put the
powder in the center of the circular sample older and if there is also
some tricks in order to avoid electrostatic problems.
Thank you very much in advance,
--
*********************************************************************************************
Pr. Francois GOUTENOIRE
e-mail:francois.gouteno...@univ-lemans.fr
Tel: 02.43.83.33.54
FAX: 02.43.83.35.06
Département des Oxydes et Fluorures
Institut des Molécules et des Matériaux du Mans
IMMM - UMR CNRS 6283
Université du Maine - Avenue Olivier Messiaen
F-72085 Le Mans Cedex 9
FRANCE
*********************************************************************************************
Formation Rietveld CNRS
https://cnrsformation.cnrs.fr/stage.php?stage=17082
Formation SASX CNRS
https://cnrsformation.cnrs.fr/stage.php?stage=17228
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++