There should be no damage but you may see a slit change in color where the beam hits the sample, a temporary change in the color center. I suggest running your generator at 45 kV and 35 mA you will get more intensity.
Cheers, Ed On Sun, May 21, 2017 at 12:21 PM, Shay Tirosh <stiro...@gmail.com> wrote: > Dear Rietveldrs > > Do you know any damaging to sample that may happen during long scanning > time say (3h). > Specifically in case the x-ray source is Cu with Ka1+Ka2 that operates > under 40mA and 40kV and the sample is metal oxides > > Please suggest on ref or book that elaborate on this topic. > > Thanks > > Shay > > > > > -- > _________________________________________________ > > Dr. Shay Tirosh > Institute for Nanotechnology & Advanced Materials > Bar Ilan University > Ramat Gan, 52900 > Israel > Phone: +972-(0)30-531-7320 > Mobile: +972-(0)54-8834533 <+972%2054-883-4533> > Email: stiro...@gmail.com > _________________________________________________ > > ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ > Please do NOT attach files to the whole list <alan.he...@neutronoptics.com > > > Send commands to <lists...@ill.fr> eg: HELP as the subject with no body > text > The Rietveld_L list archive is on http://www.mail-archive.com/ > rietveld_l@ill.fr/ > ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ > > > -- Dr. Edward A. Laitila Senior Research Engineer/Scientist II/Adjunct Assistant Professor Michigan Technological University Dept. of MSE Room 628 M&M Building (906) 369-2041
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ Please do NOT attach files to the whole list <alan.he...@neutronoptics.com> Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/ ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++