In 1953 English paper-makers J. Barcham Green Ltd issued a modest booklet 
describing in detail the process of making paper at their Hayle Mill – a small 
but valuable historical record of actual practice. A thousand copies were 
printed on Barcham Green papers but, perhaps because of its somewhat ephemeral 
nature, it is seldom seen. It was reprinted in 1960 and again in 1967 in 
slightly varying forms, but in this reprint Old School Press have returned to 
the original text. The booklet was produced for the mill’s customers and 
contains much of interest for conservators.

 

Whilst the press has not tried to produce an exact facsimile of the booklet, 
they have followed the flavour of the original in structure and typography. So, 
in particular, the cover carries the title and the delightful silhouette of the 
vatman that appeared on the cover of the original.

 

The text was written by John Barcham Green and is splendidly detailed in its 
description of the process, and in a style almost like that of Moxon describing 
printing processes in his Mechanick Exercises. As such it is an important 
authoritative text by one of England's greatest paper makers.

 

The original 1953 edition included sixteen photographs of the process as 
described, showing workers at the mill, poised at the various stages – at the 
vat, couching, drying, etc. – but they were small and not ideally printed as 
half-tones. With the kind help of Simon Barcham Green, the press has been 
fortunate to have had access to better prints of the photographs and these have 
been scanned for giclée printing at the press on their eight-colour Epson 3800 
printer. The original booklet was somewhat constrained by the small amount of 
space available, so some photographs were severely cropped thereby losing 
interesting detail, and then printed at a small scale. For the reprint Old 
School Press printed the entire original photograph in each case, without 
cropping, on an A5 (210 x 148mm) sheet of Hahnemühle Photo Rag Baryta.

 

The text of the booklet has been printed on Barcham Green's Finale paper – it 
was the last paper made at the mill before it closed in 1987 – and the cover on 
their Chatham Royal. Both papers were damped for printing. The text makes 
twenty pages and has been printed in 12pt Monotype Caslon with the titles in 
various sizes of Caslon Old Face from the Stephenson Blake foundry. The binding 
takes the form of a simple case covered in Barcham Green's Antique Rose, with a 
pocket on the inside of each board, one holding the booklet and the other 
holding the sixteen photographs loose together with a sheet of captions. The 
case is 280mm by 175mm, the booklet 260mm by 160mm.

 

The edition consists of 130 copies of which 100 are for sale. Copies are £105 
(€125, US$140) each. (ISBN 978 1 899933 42 6) For full details, visit 
http://www.theoldschoolpress.com/.

 

 

Regards

 

Simon Green

 

******
Unsubscribe by sending a message to [email protected]
Searchable archives: http://cool.conservation-us.org/byform/mailing-lists/cdl/

Reply via email to