Dear list-members,
we recently have done some oddy tests of different nitrile gloves. All results 
were very similar we do see some changes on all lead and cupper coupons. That 
means that the glove materials emit tarnishing pollutants under accelerated 
conditions. Does it also mean that in direct contact the gloves transfer 
tarnishing residue to object surfaces? Does anybody know alternatives to 
nitrile gloves? Has anybody done research on this topic?
Thanks Johanna