ICON Scotland are delighted to welcome experts from Germany for a unique 2 part 
conservation seminar inside the stunning setting of Stirling Castle:

9.30 - 12.30 : IBZ Salzchemie (Prof. Dr. Gerald Ziegenbalg & Dr Claudia 
Dietze): 'Nanolime for the consolidation of stone, mortar, plaster and wall 
paintings'
The workshop is divided into 4 topics. The first two parts deal with the basic 
properties and characterization of nanolime (CaLoSiL) and the carbonisation 
process. In addition to application notes, strategies are also discussed to 
avoid remaining white haze. In the third part the combination of nanolime and 
silicic acid ester is discussed. This is followed by various application 
examples for the consolidation of stone, plaster, mortar and wall paintings as 
well as special application areas like anti moulding agent, realkalization of 
concrete, bone and wood conservation etc.. Finally the possibility of modifying 
injection grouts and repair mortars, slurries and fillers is discussed.

13.30 - 16.30: fokus GmbH (Gunnar Siedler): 'Digital Image Rectification and 
Mapping with metigo MAP Software'
Metigo MAP is used for image rectification and digital mapping for conservation 
projects and 3-dimensional object documentation. Conservators in almost any 
speciality can benefit from the ability to produce accurate maps of two or 
three-dimensional objects. Areas of damage, treatment, or sampling can be 
precisely described and located. This course offers an introduction to 
true-to-scale mapping based on rectified digital images. Basics of digital 
image rectification, building of mapping projects, design of legends and text 
fields, and the use of drawing tools will be taught. The training uses real 
life examples and each participant should bring a laptop computer able to run 
Microsoft Windows, with a display resolution of at least 1024x768. A trial 
license for the software metigo MAP will be provided to all participants for 
the training free of charge.

Early booking is recommended as the workshops are limited to 20 participants!
Tickets: 
https://www.eventbrite.co.uk/e/icon-scotland-masonry-consolidation-conservation-mapping-seminar-tickets-63296978968

Christa Gerdwilker ACR
Chair - ICON Scotland
Email: [email protected]




Historic Environment Scotland - Scottish Charity No. SC045925
Registered office: Longmore House, Salisbury Place, Edinburgh, EH9 1SH

________________________________

This e-mail does not form part of any contract unless specifically stated and 
is solely for the intended recipient.
Please inform the sender if received in error.

________________________________
******
Unsubscribe by sending a message to [email protected]
Searchable archives: http://cool.conservation-us.org/byform/mailing-lists/cdl/

Reply via email to