Re: Can anyone recommend an appropriate consolidant and application method for 
dried plant material (looks like sphagnum moss) that makes up part of a 
composite artifact?...

Hi Dee,

A seed and nut wreath with shedding sphagnum moss elements was treated at CCI 
in 2011. The moss was consolidated with a 0.5% gelatin solution applied with an 
ultrasonic mister.

Good luck.
Amanda