I presume you're talking of the stranded stuff.  Some of that is poorly made. 
Years ago, I had a number of wire antennas fail because the strands rubbed
each other in the wind, scraping off the thin coating coating, then rusting. 
After that, I went with solid or insulated, stranded copperweld.

Barry W2UP



--
View this message in context: 
http://elecraft.365791.n2.nabble.com/OT-Handling-Copperweld-wire-tp7626383p7626423.html
Sent from the Elecraft mailing list archive at Nabble.com.