Hello all,

I am hoping to push processing some 7266 by one stop.

Usually I develop 7266 in a lomo tank using D19 + Potassium Thiocyanate as
my first developer for 6 minutes at 20 degrees Celsius. I agitate for 10
seconds each minute.

Does anyone know how I might alter the time or temperature of my first
developer to push one stop? Any guidance in terms or approximate time or
temperature increase would be greatly appreciated.

Thanks so much,