in another thread I proposed flex-seal good to 300 - 350 degrees C.  I 
don't know anyone who's tried it though.

On Tuesday, September 17, 2013 2:45:51 PM UTC-5, Frank H wrote:
>
> Thanks, Zig.
>
> Does anyone have any other suggestions, cautions or comments?
>
> - Frank
>
> On Monday, September 16, 2013 11:04:28 AM UTC-7, Zig wrote:
>>
>> I think roofing compound would be an exceedingly problematic idea here, 
>> since it will become soft if heated at all....
>>
>> If you wanted to apply a flexible coating to the edges, I would look at 
>> liquid latex, or something similar!
>>
>>
>> On Mon, Sep 16, 2013 at 10:17 AM, Frank H <[email protected]> wrote:
>>
>>> Has anyone tried using roofing compound, roofing patch, or any type of 
>>> paint for sealing the edges of isocyanate foam boards prior to joining with 
>>> tape or vinyl hinges?
>>>
>>>  -- 
>>> You received this message because you are subscribed to the Google 
>>> Groups "hexayurt" group.
>>> To unsubscribe from this group and stop receiving emails from it, send 
>>> an email to [email protected].
>>> To post to this group, send email to [email protected].
>>> Visit this group at http://groups.google.com/group/hexayurt.
>>> For more options, visit https://groups.google.com/groups/opt_out.
>>>
>>
>>

-- 
You received this message because you are subscribed to the Google Groups 
"hexayurt" group.
To unsubscribe from this group and stop receiving emails from it, send an email 
to [email protected].
To post to this group, send email to [email protected].
Visit this group at http://groups.google.com/group/hexayurt.
For more options, visit https://groups.google.com/d/optout.

Reply via email to