Dear Monica,

the file you attached does not look like an ASCII file. Anyway, usually the information you need to convert the steps into useful physical units (degree-> energy) is in the header of the files in thew Lytle database. Often not in a very clear form if I remember correctly...

You might however have a look here if you find what you are looking for, I am sure there is a Ti-foil spectrum in the database:

http://ixs.iit.edu/database/

Cheers,

Edmund


On 06.07.21 16:29, Monica Bairagi wrote:
Hello all:
I am looking forward to standard metal foil data of titanium.
I downloaded the data from the Farrel Lytle database but I can not import it 
into Athena. I looked into the data, it looked wired for me. As Athena expects 
data to be in columns of energy but this data is not recorded by energy but by 
steps of the monochromator rotation stage.
I am wondering if anyone has any idea how to import or transfer the data.
I am attached herewith the data file.
Thanks
Monica Bairagi
Ph.D. Student, Ujjain, India

_______________________________________________
Ifeffit mailing list
Ifeffit@millenia.cars.aps.anl.gov
http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
_______________________________________________
Ifeffit mailing list
Ifeffit@millenia.cars.aps.anl.gov
http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit

Reply via email to