Hi all,
I am dealing with in-situ battery measurements.
While I am changing the voltage, the white line of TM is changing its
position and intensity.
The change in intensity can be related to the order as pointed out here:
https://pubs.acs.org/doi/10.1021/acsami.0c13161
But what about energy shifts when there is no change in the oxidation
state? Any reference where to dig?
Best regards.