Hi Jerry,

I've seen people use various Li ion battery materials, lithium is nice, but
doesn't work here. Maybe NMC811 would work, it is unstable to exposure to
air and moisture. You could try some iron powder from a hand warmer pouch,
it will oxidize from ambient oxygen.

-Lyle

On Wed, Feb 21, 2024 at 1:35 PM Gerald T. Seidler <[email protected]> wrote:

> Dear XAFS community, We've been developing air-sensitive sample cells for
> several of our XAFS experiments, but we don't have a good way of
> characterizing how well they actually reject air and water.   Does anyone
> have recommendations
> ZjQcmQRYFpfptBannerStart
> This Message Is From an External Sender
> This message came from outside your organization.
>
> ZjQcmQRYFpfptBannerEnd
> Dear XAFS community,
> We've been developing air-sensitive sample cells for several of our XAFS
> experiments, but we don't have a good way of characterizing how well they
> actually reject air and water.  Does anyone have recommendations for easily
> available 3d transition metal compounds that have a 'reasonable' amount of
> air sensitivity for purposes of sample call validation?  Any suggestions
> for other methods to validate performance? We would grind the sample and
> form a pellet with a degassed binder, in a glovebox or glovebag.
> With thanks,
> Jerry
>
> --
> *Gerald Seidler*
>
> *Professor, Physics Department*
> *University of Washington*
>
> *https://urldefense.us/v3/__http://faculty.washington.edu/seidler/index.html__;!!G_uCfscf7eWS!eCvwFZmmEN_zoBONeI22H7RJ39nNzDl6pbZj4vkJCHaJ0xWs421UWvBpxrAzEo6deyBK4Ru3ctPb4DRaFuwvCoC9HkR5$
>  
> <https://urldefense.us/v3/__http://faculty.washington.edu/seidler/index.html__;!!G_uCfscf7eWS!bc8I7gtiYjYV5xc8tbm1xHCOWp8emLi4nZo7rvTjsDdGw3JMBVgas9avdYSiT995CKzLi-eu2GCc0RfkE-Cz2uX2VeU-3A$>*
> *[email protected] <[email protected]>*
> _______________________________________________
> Ifeffit mailing list
> [email protected]
> https://urldefense.us/v3/__http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit__;!!G_uCfscf7eWS!eCvwFZmmEN_zoBONeI22H7RJ39nNzDl6pbZj4vkJCHaJ0xWs421UWvBpxrAzEo6deyBK4Ru3ctPb4DRaFuwvClsh2CUj$
>  
> Unsubscribe: 
> https://urldefense.us/v3/__http://millenia.cars.aps.anl.gov/mailman/options/ifeffit__;!!G_uCfscf7eWS!eCvwFZmmEN_zoBONeI22H7RJ39nNzDl6pbZj4vkJCHaJ0xWs421UWvBpxrAzEo6deyBK4Ru3ctPb4DRaFuwvCmOgTKB2$
>  
>
_______________________________________________
Ifeffit mailing list
[email protected]
http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit

Reply via email to