Good points on T88
You convinced me on KR building to use the T88 ahead of the West.
My point was that not to worry if you used West. A pure West System
epoxy as an adhesive is not near as good as West with a proper filler,
but is as good as any epoxy adhesive if used with the proper filler and
West System recipe. I too had thermal problems on large areas...but then
when it got cold.....it would not harden properly, probably like any 2
part epoxy.
Gary

-----Original Message-----
From: [email protected] [mailto:[email protected]] On
Behalf Of [email protected]
Sent: January 25, 2006 5:20 PM
To: KR List
Subject: KR> love those resins

Maybe my mileage isn't the same.  I began construction 15 or so years
ago.  I started with the first batch of T88 taking 4 or 5 scrap pieces
from the same wood used in the project, ...... 
The T88 has a non-critical mix.  You can also mix very small batches if
you miss the mark. The West System you need to measure carefully. The
pumps are set for a fairly large batch when gluing (an incredibly small
batch when glassing something like a wing)

Paul
Derry NH

_______________________________________
Search the KRnet Archives at http://www.maddyhome.com/krsrch/index.jsp
to UNsubscribe from KRnet, send a message to [email protected]
please see other KRnet info at http://www.krnet.org/info.html




Reply via email to