Mark Langford wrote>
...With vinylester in a hundred degree hangar, things have to
happen in a big hurry!  ...but consider that vinylester under these 
conditions becomes completely
unworkable after 6-8 minutes, and hard as a rock in fifteen.  I hate the
stuff, but it was designed to line ethanol-based auto fuel tanks at your
local Zippy Mart...
+++++++++++++++++++++++++++++++++++++++++++++
The catalyst to activate the vinylester resin can be adjusted for the 
ambient temperature; use more or less catalyst: 0.5 cc catalyst per 8 oz 
resin for 20 minute working times at 100 degrees F versus 3 cc catalyst per 
8 oz at 60 degrees F.  The manufacturer's info sheet has the call-outs.

Sid Wood
Tri-gear KR-2 N6242