I was gluing something with some T-88 I bought several years ago, and part
B (the hardener) had become so thick that it wouldn't come out of the
bottle.  Finally I heated it in my microwave until it was liquid, then
mixed them as usual.

Is this acceptable practice and does it weaken the final bond?  This wasn't
for a critical joint, but I do make those sometimes, so if heating T-88
before mixing weakens the bond, I guess it's time to throw it out and buy
fresh.