I could only find the structure parameters for Cs2Si2O5 in our reasonably updated ICSD database. I wonder if there are any published structure data out there. Good luck. Tao 10/30/98 On Fri, 30 Oct 1998, Hongwu Xu wrote: > Dear All: > > Does anyone have structural information (space group, cell > parameters, atomic positions) of Cs2SiO3? The thermodynamic data for this > compound are available but I couldn't find any crystallographic info.. > > Thanks, > Hongwu Xu > >
- Cs2SiO3 Hongwu Xu
- Re: Cs2SiO3 Tao
- Re: Cs2SiO3 Alan Hewat, ILL Grenoble