At 13:25 29.01.99 +0100, you wrote:
>Dear all
>
> I am working with a Philips PW-1800 diffractometer and I want to do
>Rietveld's refinament by BGMN code.
>
> I need some variables of it; as goniometer radius, height and width
>of the X-ray tube�s focus, radius and width of the horizontal divergence
>slit, divergence angle of the primary collimator, radius and width of the
>vertical divergence slit, divergence angle of the secondary collimator,
>width and height of the detector slit, radius of a secondary
monochromator....
>
>Can anybody help me?
>
Hi Angel Luis,
please specify the tube (type) and the additional equipment (automatic
divergence slit or none). On monday we will send a *.sav file for
calculating the geometry profiles.
Best
Reinhard Kleeberg
[EMAIL PROTECTED]