On Tue, 16 Feb 1999, Alan Hewat, ILL Grenoble wrote:

> >C4A3S is the 'precursor' for
> >ettringite formation and is added to Portland cement to produce shrink-
> >compensated, fast-setting concrete. 
> 
> Now that I have drawn the structure it looks interesting :-)  6-member 
> rings of corner connected AlO4 tetrahedra with Ca in the center, and the
> rings connected to form large cavities containing the sulphate. Wulf Depmeier
> et al. had it cubic, while the recent x-ray Rietveld work of Colin Kennard 
> et al has it othorhombic pseudo-cubic.  
> 
Y. G. Wang et al. did an electron diffraction study on it which revealed
superstructure reflections (J. Mater. Sci. Let. 9 (1990) 997).

Is the article of Kennard published already? I could not find it with
UnCover.
 

> It would perhaps be interesting to do some neutron work on this material
> to see if there is no hydration in all those cavities, n'est pas Colin ?
> 
Maybe in the material found in cement, but most of the material for
studies is prepared from CaO and Al2O3 without any water or hydroxides
involved in the process.


***********************************************************************
Daniel M. T�bbens                                Tel.: +49 30 8062-2793
Hahn-Meitner-Institut                            Fax : +49 30 8062-2999
Glienicker Stra�e 100
D-14109 Berlin, Deutschland          http://www.hmi.de/people/toebbens/
***********************************************************************


Reply via email to