Hi!
In GSAS or FULLPROF
if one wants to refine occupany of two atoms occupying the same site ,
use the codes 1 -1 for example(constraint number and negative of that).
What I am interested, is to know how to use the codes
if I have more than two atoms in the same site (either in GSAS or FULLPROF)?
Could some one suggest me how to go about refining
with more than two atoms in one site?
Thanks
kasthuri
--