On 05/26/99 Angel Luis Ortis Seco wrote: Oggetto: Sol-gel SiC

>Dear all,
>I would like to know some referents about sol-gel applied to SiC.

Dear  Angel,

Concerning the sol-gel method for production of SiC you can read :

Laine R., Babonneau F. "Preceramic polymer routes to silicon carbide" Chem.
Mater. 5 (1993) 260-279

Schmidt W.R., Interrante L.V., Doremus R.H., Trout T.K., Marchetti P.S.,
Maciel G.E. "Pyrolysis chemistry of an organometallic precursor to silicon
carbide" Chem. Mater. 3 (1991) 257-267

I am involved in XRD characterisation of Si-C-O compounds obtained by
sol-gel techniques, so you can contact me for further discussion.


Herv�

----------------------------------------------------------------------------
------
Dr Herv� Brequel
Dipartimento di Chimica
Via Vienna 2
I-07100 Sassari, Italy

Tel : (+39)-079-229524
Fax: (+39)-079-212069
e-mail: [EMAIL PROTECTED]
----------------------------------------------------------------------------
------