Daniel M. Toebbens wrote:
>
> Does anybody know about a good calibration standard which can be
> used for peak shape control in the low angle region in neutron powder
> diffraction? Low angle meaning 2Theta = 5� - 20� with a wavelength of
> 1.6Ang -- a d-range of 20 Ang - 4.5 Ang. In this region the material
> should have a few a) strong and b) well resolved reflections.
R. Gilles, U. Keiderling and A. Wiedenmann, "Silver behenate powder as a
possible low-angle calibration standard for small-angle neutron
scattering", J. Appl. Cryst. 31 (1998), 957-959.
> Daniel Toebbens
>
> ***********************************************************************
> Daniel M. Toebbens Tel.: +49 30 8062-2793
> Hahn-Meitner-Institut Fax : +49 30 8062-2999
> Glienicker Strasse 100
> D-14109 Berlin, Deutschland http://www.hmi.de/people/toebbens/
> ***********************************************************************
--
Jacco van de Streek (mailto:[EMAIL PROTECTED])
http://www.caos.kun.nl/cmsc/