Dimitri,
Boy all these diffractometers that can't do steps properly! Yes, the "ALT"
format is the right way to read the data. Use "CONST" for the bintyp and
start & average step for BCOF(1) & (2). These are in deg*100. For the data
there are 3 columns. The first is 2-theta*3200, second is intensity & third
is the esd for the intensity.
Bob
At 12:37 PM 2/9/00 -0600, you wrote:
>Bob,
>
>I have some APS data taken with somewhat of an eratic step size.
>I wish to make a data file for GSAS with 2theta and count to take care of
>this problem.
>
>is the header
>
>('BANK',3I,A,4F,' ALT')IBANK,NCHAN,NREC,BINTYP,(BCOEF(I),I=1,4)
>
>the best way to do this ? What would you suggest ?
>
>best,
>Dimitri
>
>--
>Dimitri N. Argyriou
>Materials Science Division
>Argonne National Laboratory
>9700 South Cass Ave.
>Argonne, IL, 60439
>Phone: (630) 252 5541
>Fax: (630) 252 7777
>Email: [EMAIL PROTECTED]
>
>> From: [EMAIL PROTECTED] (Bob Von Dreele)
>> Reply-To: RIETVELD_L Distribution List <[EMAIL PROTECTED]>
>> Date: Fri, 04 Feb 2000 08:47:45 -0700
>> To: RIETVELD_L Distribution List <[EMAIL PROTECTED]>
>> Subject: Re: Absorption GSAS and TOF Instruments
>>
>> Dear Jon,
>>> PS: Can anyone tell me if sigma_abs goes as 1/v for Gd?
>> No. It's a lot different from that. You might be interested to know that
>> I'm working on getting b' & b" for such isotopes & elements into GSAS.
>> Bob Von Dreele
>>