GSAS now contains a function that is appropriate for quite highly absorbing 
samples. However, it is not documented in the manual. Have a look in your 
version of GSAS and see if it is there. If not get the latest GSAS release.

                                                         Angus



At 08:16 PM 2/17/00 -0500, you wrote:

>         Should I concern myself about X-ray absorption in Rietveld refinement
>and sturcture solution from powder data?  If so, is there way to input mass
>attenuation coefficients into GSAS?  I have read page 123 of the GSAS 
>TECHNICAL
>MANUAL and seems to say no.  The Debye-Scherrer absorption function is
>suggested only for "a weak absorber" and seems to be an arbitrary function
>derived from neutron diffraction.  The other functions are inappropriate 
>for my
>experimental conditions.  Should I just refine thermal parameters, which are
>presumed highly correlated with absorption, and not worry about it?
>
>I am working with a strongly absrobing material, CuAlI4 in a Debye-Scherrer
>geometry.  I have used mucalc, on Brian Toby's NIST website
>
>http://www.ncnr.nist.gov/programs/crystallography/mucalc.html
>
>as earlier suggested by Lachlan Cranwick on this list.
>
>Using the crystalographic density,  Packed density = 6.673 (g/cc)
>Wavelength = 0.9388 (A)
>
>mu = 497.8 cm-1
>
>Using 0.6 the crystalographic density,  Packed density = 4.003 (g/cc)
>Wavelength = 0.9388 (A)
>
>mu = 298.6 cm-1
>
>Thank you for any experience in this matter.
>
>Roger
>
>