In a message dated 4/3/00 12:59:08 PM Pacific Daylight Time, [EMAIL PROTECTED] writes: << The maximum count was 17,500 cps and lobes were observed at about 15 cps >> This is actually pretty good focussing for powder diffraction application; the focal to satellite intensity ratio for this tube has improved by a factor of ~10 compared to what Bergmann reports. Question to Bergmann: With such a tube, would defocussing still matter? L. Keller
- Re: Kalpha2 Armel Le Bail
- Re: Kalpha2 Joerg Bergmann
- Re: Kalpha2 Jim Cline
- Re: Kalpha2 Armel Le Bail
- Re: Kalpha2 Diffract
- Re: Kalpha2 Joerg Bergmann
- Re: Kalpha2 Diffract
- Re: Kalpha2 Joerg Bergmann
- Re: Kalpha2 Jim Cline
- Re: Kalpha2 Joerg Bergmann
- Re: Kalpha2 Diffract
- Re: Kalpha2 Dr.Joerg Bergmann