Dear Natale

In my opinnion the use of digitized data from Debye - Scherrer
film for for Rietveld Refinement is not a good selection

may be for the one very specific sample the results are goods,
but in general I think the use of good diffractometer is
a GOOD SELECTION

Best Regards

Ramon
--------------------

Prof. Ramon Pomes Dr.Sc.
X Ray Lab.
National Center for Scientific Research
p.o. Box 6880
Havana
Cuba

> 
> Dear All,
> I am planning to do Rietveld refinement starting from Debye-Scherrer film
> digitized data. Presently we use in our laboratory the "Direct Exposure
> Film" DEF 392 produced by Kodak. I am not sure this is the best choice for
> my purpose, so I would like to know which kind of materials people use. 
> Best Regards            Natale Perchiazzi
> �����������������������������
>                Natale Perchiazzi                           
>   Dipartimento di Scienze della Terra 
>        Universit� degli Studi di Pisa           
>      Via S.Maria 53, I-56126 Pisa        
>              tel +39 050 847269                         
>              fax +39 050 500932                       
>       e-mail [EMAIL PROTECTED]                
> �����������������������������
> 

Reply via email to