As implied from the previous Email, there is a Scott Belmonte GSAS friendly
utility called "coue" (GPL'd).
This converts Crystals LIST 16 bond restraint files to GSAS macro format
and Bruker Topas Rietveld format. It is made available with Source code,
Windows executable and is released under the Gnu Public Licence so can be
freely redistributed and modified for extra functions and extra Rietveld
formats.
http://www.ccp14.ac.uk/ccp/web-mirrors/scott-belmonte-software/
Lachlan.
--
Lachlan M. D. Cranswick
Collaborative Computational Project No 14 (CCP14)
for Single Crystal and Powder Diffraction
Daresbury Laboratory, Warrington, WA4 4AD U.K