In the study of non-expansive, fast-setting calcium-sulfo-aluminate based clinker materials, has anybody come across a fluorine bearing phase which is vaguely described as 'calcium-fluoride-silicate-sulfate'? It supposedly forms at certain burn conditions in production kilns. L. Keller
- Re: Cement Clinkers Diffract
- Re: Cement Clinkers Jens Wenzel Andreasen