Dear colleagues,

I have data collected in a Bruker diffractometer D8 in variable divergent
slits V6/V6, I would like to correct the data by using the ICORR variable
and the file COR.COR in the program FULLPROF. Does anyone have use this
option ? it seems that it does not work.

My file for the correction is below :
Fichier de correction V6/V6 I(FDS)=correction*I(VDS)
         5.00   2.063901
        10.00   1.035891
        15.00   0.695004
        20.00   0.525933
        25.00   0.425630
        30.00   0.359757
        35.00   0.313607
        40.00   0.279838
        45.00   0.254382
        50.00   0.234809
        55.00   0.219584
        60.00   0.207697
        65.00   0.198463

Thanks