On Tue, 6 Mar 2001 [EMAIL PROTECTED] wrote: > Have a documented c-value of 5.178A for stoichiometric, hexagonal GaN (PDF > card #2-1078); can anybody confirm this value and its uncertainty or are > there updated and/or more precise c-values for GaN (Ga:N=1) available? > > L. Keller > We have done Rietveld refinement on GaN powder obtained by grinding single crystals and the results were the following: a=3.1843(5) c=5.1746(8) Stan [EMAIL PROTECTED]