Title: PDF Workshop
By adding a known concentration of a crystalline internal standard, and doing a Rietveldr efinement, you can quantify the crystalline phases, and the amorphous component by difference.
-----Original Message-----
From: Anthony Manerbino [mailto:[EMAIL PROTECTED]]
Sent: Tuesday, March 20, 2001 9:23 AM
To: '[EMAIL PROTECTED]'
Subject: Unknown amorphous phase.

Hello,
 
    I am working with samples that contain an unknown amorphous phase, which I would like to quantify.  Does anyone know of any publications that might discuss some methods or techniques that may be used to determine the unknown amorphous phase. I would like to try and use a method that introduces an internal standard but I am open to all ideas.
 
Thanks,
  Anthony Manerbino

Reply via email to