Dear Ortiz,
The complete reference is as follows:
Dollase, W. A.; Reeder, R. J.. Crystal structure refinement of huntite,
CaMg3(CO3)4, with x-ray powder data. Am. Mineral. (1986), 71(1-2),
163-6. CODEN: AMMIAY ISSN:0003-004X. CAN 104:71944 AN 1986:71944
CAPLUS
Hope this will help you.
Regards
Akash
On Wed, 30 May 2001, Angel L. Ortiz wrote:
> Dear all,
>
> Could somebody tell me the full reference of the following paper?:
>
> W.A. Dollase and R.J. Reeder, Am. Min., 71 163 (1986).
>
> Please, note that I am interested in the whole tittle of that paer as well
> as the final page. I need to give it as a reference.
> Thanks in advance.
>
>