> Who know the atom fractional coordinates of Li2SnO3?
there is some confusion about the correct coordinates in the
old (1954 Lang, Z. Anorg. Allg. Chem.) literature.
the correct values are:
TITL Lithium stannate
TITL Li2 Sn O3 Die Kristallstruktur von Li2SnO3 Kreuzburg G Stewner F Hoppe R
TITL Z. Anorg. Allg. Chem.
CELL 1.54178 5.29500 9.18400 10.03200 90.000 100.130 90.000
C 2/C
Li1 0.23900 0.07800 -0.00100 1.0 0.01
Li2 0.25000 0.25000 0.50000 0.5 0.01
Li3 0.00000 0.08300 0.25000 0.5 0.01
Sn1 0.00000 0.41650 0.25000 0.5 0.01
Sn2 0.00000 0.75080 0.25000 0.5 0.01
O1 0.13370 0.25970 0.13330 1.0 0.01
O2 0.11020 0.58440 0.13420 1.0 0.01
O3 0.13460 0.90920 0.13290 1.0 0.01
caroline.