On 5 Sep 01, at 10:43, stefano agrestini wrote:

> Dear all,
> Could anyone give me the x-ray scattering factors values for B-1 ? Is
> fundamental for the Rietveld analysis of my x-ray powder diffraction
> data.
> Thank you very much
>
> Dr. Stefano Agrestini
>
>
> "La Sapienza" University of Rome
> Physics Department
> e-mail : [EMAIL PROTECTED]

the International Tables for Crystallography Vol 3 (1962) Kynoch
Press give X-ray scatt factors for boron(1+).
this helps?

Miguel Gregorkiewitz
Dip Scienze Terra, Universit�
via Laterina 8, I-53100 Siena, Europe
fon +39'0577'233810 fax 233938
e-mail [EMAIL PROTECTED]