Ozhan Unverdi wrote:

Could someone give me the magnetic scattering factors of Ru+4 please?


www.google.com searching for "Ru4+ magnetic form factor" gives 17 results.

One of them is Sidis et al, "Evidence for Incommensurate Spin Fluctuations in Sr2RuO4", Phys. Rev. Lett (1999) 83, 3320.

In that paper they say: "The intensity of the scattering can be reasonably well described by the squared magnetic form factors of the Ru+ ion [19] (note that the magnetic form factor is Ru4+ is not available)". Ref 19 is international tables vol C.

So it seems unlikely that anyone is about to give you the 8 numbers you seek, although that paper is five years old. You could try plotting out the Ru+ form factor and squaring it to get an approximation to the Ru4+ form factor. Or you could try to do it analytically if you know what the 8 numbers mean, I'd guess at sum of A(I)*exp(-B(I)*SQ) for I=1 to 4 with SQ=sin(theta/lambda)**2, and no constant term based on what GSAS uses. It would probably be a good idea to try testing all of Ru, Ru+ and (Ru+)**2 form factors too see if there is any difference in the results.

Going further into the google results you might also want to read Gukasov et al, Phys. Rev. Lett (2002) 89, 087202. They seem to discuss the form factor of Ru in Ca1.5Sr0.5RuO4 quite extensively.

Good luck!

Jon