Dear Rietvelders, I used GSAS to refine my structure in P2/n, however the program automatically fixed the the XYZ positions of the first atom during refinement. To my surprise, this atom is not seen in the "fixed atom list" in the atom parameters menu of GSAS.
Please advise and many thanks, stephen