Ana (& others), Find this option in the print options in the least squares control menu. The output will list only those covariance terms >0.50 and <-0.50 (i.e. just the big ones). It is a very condensed table with a variable name followed by variable names & covar. value. Bob Von Dreele
________________________________ From: Ana Isabel Becerro [mailto:[EMAIL PROTECTED] Sent: Mon 4/12/2004 5:41 AM To: [EMAIL PROTECTED] Dear all, I would be very grateful if you could tell me how to see the correlation matrix in a Rietlveld refinement with GSAS. Thanks a lot! ana Dr. Ana Isabel Becerro Departamento Qu�mica Inorg�nica Instituto de Ciencia de Materiales de Sevilla Universidad de Sevilla-CSIC Tel: +34 954489576 Fax: +34 954460665