Here are the codewords for two parameters I set in the file *.pcr,
             0.14854  0.29708
              291.00   292.00 
the result in the file *.sum is:
         x     sx       y     sy  
      0.14488( 911)  0.28976( 911)
why these two standard deviations are the same? The second should be twice
as large as the first, and also in the "Mathematical Information" of the manual
it said the coefficient of the codeword would be multiplied.
so who could tell me the reason?
 
Thanks in advance!
-----------
Zhijian Fan                
E-mail: [EMAIL PROTECTED]                 
 
 

Reply via email to