However, I maybe personally suggest to try this software at the address, A simple 
program for analyzing the diffraction line broadening is available. The program 
calculates domain size and strain from input integral breadths of at least two 
physically broadened diffraction-line profiles.:
http://www.boulder.nist.gov/div853/balzar/breadth.htm









Best Regards,
Lingfei Zhang
*****************************************
Neutron Scattering Physics Group
Institute for Materials Research
Maxwell Building 111
University of Salford
Salford, Greater Manchester
United Kingdom M5 4WT
Tel:0161 295 4633
Facsimile:0161 295 5147
Email:[EMAIL PROTECTED]
*****************************************

Reply via email to