On Thu, 06 May 2004 16:56:44 +0200, Robert Mauricot wrote: >Dear all, > >I have a powder diffraction of an amorphous multiphase material. I want to >do a quantitative analysis of the amorphous phase. Can anyone tell me what >software does it.
Many Rietveld programs will do so. For example, BGMN comes with an example for amorphous estimation, see www.bgmn.de/download.html -> www.bgmn.de/download/amorph.zip The principle is using an internal standard of known content. >Sincery J"org Bergmann, Dresden [EMAIL PROTECTED] *** This EComStation system uptime is 2 days 0 hours ***