Namsoo,
Robert
Dinnebier has an extensive list of materials and their transition points (some
solid-solid phase transitions, some melting) on his web-site
at:-
Alternatively, the book "X-ray Diffraction at Elevated Temperatures"
Chung, deHaven, Arnold, Ghosh, VCH Publishers, ISBN 0-89573-745-0 has a less
extensive list on page 148.