since zeolite X is cubic I do not think that you will have any problems with preferred orientation! Just sit back, relax and enjoy the beautiful structure ;-)
Best
Christian Baerlocher
On May 30, 2004, at 9:38 PM, fatiha belarbi wrote:
Dear All,------------------------
Could you please advise me how must prepare my powder to obtain a pattern without preferentiel orientation.
My sample is a zeolite X exchanged
I'm going to do a strucutre resoltion and its affinmey using the Rietveld commercial software
With many thanks for your help and best regards,
�
Ouassyla