Hi Apu,
About your question: "In this case it is case it is expected that there
will be formation of dislocation loops in the material due to
irradiation".

You may want to read:
Barabash, R., and Krivoglaz, M. (1982). On the theory of x-ray and
thermal neutron scattering by strongly distorted crystals with
dislocation loops. Metallofizika 4, 417-428.
It is in Russian but you may find the translation of the journal into
English.
You may also read a book Krivoglaz, M. (1996). X-ray and neutron
diffraction in nonideal crystals (Springer Ver-lag, Berlin-NewYork).

Hope it helps,
Rosa 

-----Original Message-----
From: [EMAIL PROTECTED] [mailto:[EMAIL PROTECTED] 
Sent: Tuesday, June 01, 2004 12:15 PM
To: [EMAIL PROTECTED]


Dear All,
I am trying to analyze the XRD pattern from an irradiated (irradiated
with high energy heavy ion) material.There are considerable amount of
broadening in the XRD peaks.In this case it is expected that there will
be formation of dislocation loops in the material due to irradiation.


Thanks in advance.

Regards,
Apu
****************************************************
Apu Sarkar
Research Fellow
Variable Energy Cyclotron Centre
Kolkata 700 064
phone: 91-33-2337-1230 (extn. 3190)
Fax:   91-33-2334-6871 
INDIA
****************************************************