Dear Rietveld users,
 
I have some difficulty to refine a structure. A double-lattice superstructure is suppose to superimpose on the orginal one, the lattice length is slightly deviated. But when I tried to do this, the refinement is poor even after I fix the fraction of the 2nd phase to be 5%. That may be because the peaks for the 2 phases are almost at the same position and it seems gsas tries to split the peak.....
Do anybody ever encounter this kind of problem? How did you solve it?
Thanks greatly!
 
Sincerely,
 
Ling Yang
Dept of CME, Univ of Cincinnati
Current address:
Bldg 8600, MS 6474
SNS, Oak Ridge National Laboratory
Oak Ridge, TN 37830
Tel: 865 574 0350
Fax: 865 241 5177