(I guess you mean the peak profile has a tail, maybe due to scattering from very thin crystallites ?) Alan.
Perhaps this is the problem because I use the SMTP server of Rennes and the POP one of Mulhouse...
Subjet: Right asymmetry
Dear all,
Following an experiment with synchrotron radiation, we noticed a compound which presents several pics with a rather strong "right asymmetry".
We think to problems of stacking faults. We would like to find some more informations about such a profil.
In particular, we are looking for a program which could be able to refine these profils correctly and we need complementary literature that what we found on the ccp14 for example. For the program we though to MarqX ?
Thanks a lot in advance for all your informations and help
Best
JM
Alan Hewat, ILL Grenoble, FRANCE <[EMAIL PROTECTED]> fax (33)
4.76.20.76.48
(33) 4.76.20.72.13 (.26 Mme Guillermet)