Dear Rietvelders,
I am working with mechanical alloying of Zr-Nb alloys system. So, I suspect 
that in same milling process I obtainded some level of anisotropic broadening.
I am working with GSAS/EXPGUI (windows version), and I want to know how to 
create and select from EXPEDT the option of principal broadening axis?
Can you help me?
SIncerely,
Sebastiao Loureiro
PhD student
Metallurgical and Materials Engineering Program
COPPE-UFRJ - Brazil

--
Metalmat Webmail (http://webmail.metalmat.ufrj.edu.br/webmail)


-- 
Esta mensagem foi verificada pelo sistema de antiv�rus e
 acredita-se estar livre de perigo.

Reply via email to