Dear all,
I have studied a compound which consist TiO2 and Fe powder. I tried to match
the xrd pattern using ICDD and ICSD, but there is no match between them.
Although the pattern looks the same, but the sin2t is too much different.
Can anyone give me a clue how to solve this problem? I had recollect the
data and the result is the same. I suppose I can�t use GSAS to analyze that.
I believe it contains more than two phases.
Another problem is I try to figure out the meaning of characters on GSAS,
List file. Anyone can help me to explain the header of GSAS LST file?
Iref H K L Mul Icod D-space Fosq Fcsq FoTsq FcTsq
Phas
1 0 0 3 2 1021 4.6372 7.076E+03 7.319E-01 5.895E+05 1.038E+02
0.0
2 1 0 1 6 1021 4.1767 1.693E+03 4.994E-01 1.411E+05 7.854E+01
180.0
Thank you for your help.
Best regards,
Riza Iskandar
Research Center for Materials Science
University of Indonesia
�